• Why heat soaking process is not recommended ?

    The Nis inside glass will cause tempered glass self explosion after installation.The glass breakage,replacement will bring numerous problems to clients,so many glass processors recommend heat soaking process after tempering to decrease the self breakage ratio. Heat soaking process is finished by heat soaking furnace,take the glass into the furnace,heating up to 300℃,keeping the temperature for 2 hours and then decrease temperature,the Nis inside glass will transfer and expand many times which can cause glass breakage,after heat soaking,the glass breakage ratio…